Stress corrosion cracks at the weld toe of the welded pipe

Posted by Mark Macharia on January 16, 2019
0

The weld toe of the welded steel pipe is easy to form stress corrosion crack. The stress concentration of the butt joint is mainly caused by the weld height, and the weld of the butt joint has the greatest stress at the weld toe. Stress concentration factor The magnitude of the stress concentration factor depends